Stacking should be done only on even and leveled ground surface

Ready made jointing chemical with 3 to 4
mm thickness or with conventional cement
mortar (1:6)

Before Application of motor dip block in
water and lift immediately or apply
water with brush

Keep it limited to 10 to 12 mm with regular cement mortar and 3 to 4 mm with ready-made jointing mortar.

Coping beam (Bond beam) with 2 nos. of 8 mm bia. reinforcement after 1.2 mts height.

Curing required only for cement mortar
joint and not required for ready made
mortar jointing.

Use tool like hacksaw or rotary cutter or
hand wood saw

Minimum 150 mm support for lintels at
both side. Lintels should be placed on
mortar bed.

MMinimum External plaster thickness 12 to 15mm.

Chases to be grooved before plastering of wall by using electrical cutter and chiseled gently without hammering to avoid damages to walls.

Wallnett AAC blocks use 65 to 70%
of fly ash, wastage generated from
thermal power plant. It does not
required clay so no damage of
agricultural land and soil.

Fly ash wastage is from thermal power
plant mixes with environment and
increase pollution, because of its use
inWallnett AAC blocks it helps to reduce
the pollution.

Wallnett AAC block are 3 times lighter than clay bricks and 4 times lighter than concrete blocks, so more number of blocks are transported in same vehicle which save fuel for transportation compared to clay bricks / Concrete blocks.

Green building certifying organization
like LEED, IGBC, BREEAM, DGNB,
CASBEE Certify AAC blocks as a green
building material.
Popular Blogs
Application of AAC Blocks

- Residential Buildings
- Commercial Buildings
- Educational Institutes
- Hotels & Restaurants
- Retail & Warehouses
- Cold Storage Industries
- Medical Clinics and Hospitals
- Firewalls & Soundwalls